Heat Cure Denture Base Material

Sale price Rs. 5,200.00 Regular price Rs. 5,800.00 10% Off
Regular price Rs. 5,200.00
Taxes included. Shipping calculated at checkout.
Inclusive of all taxes

Cash On Delivery (COD) Payment Service Available

Save Extra with 3 offers

Save Rs. 500 Discount on order above Rs 20,000

Save Rs. 200 Discount on order above Rs 10,000

Save Rs. 100 Delivery charges on orders above Rs 5,000

Description

Ivoclar SR Triplex Hot Pink V-Standard Kit
SR Triplex Hot ensures accuracy of fit and stability of shape and shade for conventional and implant supported dentures.
SR Triplex Hot is a heat-curing, PMMA-based denture base material for the condensing technique. It offers you ease of handling and your patients comfort of fit. Additionally, a veined version of the material is available

Information

  • Brand: Ivoclar
  • Key Specifications: WORKING TIME:

    As soon as the material has matured sufficiently and is no longer sticky, it can be worked for approx. 20 minutes at 23 °C / 73 °F. Dough time and working time depend on the room temperature.
  • Directions to Use: Application procedure
    Isolate boiled-out, well-wetted plaster surfaces with two layers of Ivoclar Vivadent Separating Fluid and allow to dry
    To ensure an adequate bond with the denture base, roughen the teeth thoroughly and wet them with monomer
    DOSAGE:
    Ideal mixing ratio for one denture:
    23.4 g polymer (powder) : 10 ml monomer (liquid)
    With dosage system
    1 denture
    Polymer: 2nd graduation on measuring cylinder Monomer: 10 ml
    2 dentures
    Polymer: 3rd graduation on measuring cylinder Monomer: 20 ml
    MIXING:
    Thoroughly mix polymer and monomer in the given ratio with a spatula. Leave to mature in the closed mixing cup at room temperature (23 °C / 73 °F) for approx. 10 minutes
    Polymerization
    Heat-polymerization can be carried out in two ways:
    Standard procedure (recommended method) Place closed flask in cold water, heat up to 100 °C / 212 °F and let boil for 45 minutes
    Alternative procedure Place flask in boiling water. Bring the water to the boil again and then let boil for 20 minutes. The alternative procedure is suitable only for small to medium-sized dentures. Layer thicknesses must not exceed 1 cm. The residual monomer content can be reduced by increasing the polymerization temperature and extending the polymerization time. We recommend using the standard procedure to keep residual monomer at minimum levels. If the standard procedure is used, the residual monomer content is < 2.2%
    Cooling
    Let the flask cool at room temperature for 30 minutes. Subsequently, completely cool the flask with cold water
    Deflasking and finishing
    Open the completely cooled flask and remove plaster. Check occlusion of the denture. Subsequently, finish and polish in the usual manner

Packaging

1 x 1 kg bag of polymer
1 x 500 ml monomer
1 x polymer measuring cylinder
1 monomer